Density dependence of the room temperature thermal conductivity of atomic layer deposition-grown amorphous alumina (Al2O3)
Published - Experimental (Heat Transfer)
Caroline S Gorham, John T Gaskins, Gregory N Parsons, Mark D Losego, Patrick E Hopkins
Applied Physics Letters 104.25 (2014): 253107
Publication year: 2014
External Link